Bestar Steel supplied 900 MT of API 5L Grade B SSAW steel pipes in 813 × 9 mm and 1013 × 10 mm sizes for a water conveyance pipeline project in Algeria.
Bestar Steel supplied ERW and SSAW carbon steel pipes, elbows, and forged flanges for water supply and drainage projects in Kenya, Nigeria, and Bangladesh in 2018.
Bestar Steel supplied 750 MT of 406.4 mm seamless steel pipes and fittings to ISO 3183 / API 5L PSL2 Grade L360NS (X52) for a gas transmission project in Mexico.
Bestar Steel supplied API 5CT J55 steel pipes sized 508.00 × 11.13 × 16 mm for the marine loading jetty at the Dung Quat Refinery product export port in Vietnam.
Bestar Steel supplied 3,000 tons of 42-inch API 5L X52 LSAW steel pipes with 1.25-inch wall thickness for conductor pipe piling and offshore well construction at SARB wells in the UAE.