Çelik Levha / Rulo

  • Paslanmaz Çelik Bobin

    Paslanmaz Çelik Bobin

    Tip:Paslanmaz Çelik Bobin, Çelik Bobin
    Kalınlık:0,45 mm – 5,0 mm.
    Genişlik: 914/1219/1500/2000, vb.
    Standart: ASTM A240, ASTM A480, JIS G4304, JIS G4312, vb.
    Seviye: 304, 304L, 316, 316L, 321 veya 409, 420, 430, 439, 441
    Sona ermek: 2B, No.4, BA, No.1, vb.
    Paketleme: Kenevir ipiyle birlikte paketlenmiş/Toplu halde

  • Paslanmaz Çelik Levha

    Paslanmaz Çelik Levha

    Tip:Paslanmaz Çelik Levha, Çelik Levha
    Kalınlık:5,0 mm – 50,0 mm.
    Genişlik: 1250/1500/2000 ve 2500, vb.
    Standart: ASTM A240, ASTM A480, JIS G4304, JIS G4312, vb.
    Seviye: 304, 304L, 316, 316L, 321 veya 409, 420, 430, 439, 441
    Sona ermek: 2B, No.4, BA, No.1, vb.
    Paketleme: Kenevir ipiyle birlikte paketlenmiş/Toplu halde

  • Karbon Çelik Levha

    Karbon Çelik Levha

    Tip: Karbon Çelik Levha, Çelik Levha
    Kalınlık: 5,0 mm – 50,0 mm.
    Genişlik: 1000/1200/1250/1500/1800/2000/2200, vb.
    Standart: ASTM A36, ASTM A283, ASTM A1008, ASTM A285, ASTM A515, ASTM A516, JIS G3141, vb.
    Seviye: ASTM A36, Gr. ABC D, Gr 55, 60, 65, 70, Q235B, Q355B, vb.
    Yüzey: Siyah, yağlı, boyalı, galvanizli, vb.
    Paketleme: Kenevir ipiyle birlikte paketlenmiş/Toplu halde

  • Karbon Çelik Bobin

    Karbon Çelik Bobin

    Tip: Karbon Çelik Bobin, Çelik Bobin
    Kalınlık: 1,5 mm – 6,0 mm.
    Genişlik: 914/1219/1500/2000, vb.
    Standart: ASTM A36, ASTM A283, ASTM A1008, ASTM A285, ASTM A515, ASTM A516, JIS G3141, vb.
    Seviye: ASTM A36, Gr. ABC D, Gr 55, 60, 65, 70, Q235B, Q355B, vb.
    Yüzey: Siyah, yağlı, boyalı, galvanizli, vb.
    Paketleme: Kenevir ipiyle birlikte paketlenmiş/Toplu halde