ASTM A106 pipe (also covered in ASME specifications as S/A 106) is the standard specification for seamless carbon steel pipe for high-temperature service. Most common uses are in refineries and plants when gasses or fluids are transported at high temperatures and pressures.  Bestar Steel is a world leader in the supply of A106 / SA 106 pipe and stocks a full range of grades B/C in a size rage of NPS 1/8″ to NPS 48″, with nominal (average) wall thickness as given in ANSI B36.10. Pipe having other dimensions may be furnished provided such pipe complies with all other requirements of this specification*.  Pipe ordered under this specification shall be suitable for bending, for flanging, for welding, and for similar forming operations. A full range of A106 stock is available in Schedules 10 through 160, STD, XS, XXS. Unscheduled wall thicknesses available up to 4 inches.

a106

Bestar Steel stocks a full range of A106 seamless carbon steel pipe.

 Grades B/C

 Sizes

NPS 1/8″ to NPS 48”
Wall thickness: Schedules 10 through 160, STD, XS, XXS.

*Commonly requested unscheduled walls up to 4” and certified minimum wall items

 

Chemical Properties %


C, max. Mn P, max S, max Si, min Cr, max Cu, max Mo, max Ni, max V, max
Grade A * 0.25 0.27 – 0.93 0.035 0.035 0.10 0.40 0.40 0.15 0.40 0.08
Grade B 0.30 0.29 – 1.06 0.035 0.035 0.10 0.40 0.40 0.15 0.40 0.08
Grade C 0.35 0.29 – 1.06 0.035 0.035 0.10 0.40 0.40 0.15 0.40 0.08

*For each reduction of 0.01% below the specified carbon maximum, an increase of 0.06% manganese above the specified maximum will be permitted up to a maximum of 1.35%.

 Mechanical Properties


Grade A Grade B Grade C
Tensile Strength, min., psi, (MPa) 48,000 (330) 60,000 (415) 70,000 (485)
Yield Strength, min., psi, (MPa) 30,000 (205) 35,000 (240) 40,000 (275)

(Note: This is summarized information from ASME Specification A106. Please refer to the specific Standard or Specification or contact us for more details.)

ASTM A53 Seamless Pipe

Standard Specification for Pipe, Steel, Black and Hot-Dipped, Zinc-Coated, Welded and Seamless

ASTM A53 (ASME SA53) carbon steel pipe is a specification that covers seamless and welded black and hot-dipped galvanized steel pipe in NPS 1/8″ to NPS 26.  A 53 is intended for pressure and mechanical applications and is also acceptable for ordinary uses in steam, water, gas, and air lines.

A53 pipe comes in three types (F, E, S) and two grades (A, B).

A53 Type F is manufactured with a furnace butt weld or may have a continuous weld (Grade A only)

A53 Type E has an electric resistance weld (Grades A and B)

A53 Type S is a seamless pipe and found in Grades A and B)

A53 Grade B Seamless is our most polar product under this specification and A53 pipe is commonly dual certified to A106 B Seamless pipe.

a53

Bestar Steel has a full range of stock in A53 steel pipe (SA53 steel pipe) in:

Grade B

Sizes

NPS ¼” to NPS 26” O.D.

Wall thickness: Schedules 10 through 160, STD, XH and XXH
Commonly requested unscheduled walls up to 4” and certified minimum wall items

Chemical Properties %

 GradeC,maxMn, maxP,maxS,maxCu*,maxNi*, maxCr*, maxMo*, maxV*, maxType S(Seamless) A0.250.950.050.050.400.400.400.150.08B0.301.200.050.050.400.400.400.150.08Type E(Electric-resistance Welded) A0.250.950.050.050.400.400.400.150.08B0.301.200.050.050.400.400.400.150.08Type F(Furnace-welded)A0.301.200.050.050.400.400.400.150.08

 

*The total composition for these five elements shall not exceed 1.00%

Mechanical Properties


Grade A Grade B
Tensile Strength, min., psi, (MPa) 48,000 (330) 60,000 (415)
Yield Strength, min., psi, (MPa) 30,000 (205) 35,000 (240)

(Note: This is summarized information from ASME Specification A53. Please refer to the specific Standard or Specification or contact us for more details.)

 

EN 10216-1 Seamless Pipe

Standard:EN 10216-1
Seamless steel tubes for pressure purposes - Technical delivery conditions - Part 1: Non-alloy steel tubes with specified room temperature properties

EN 10216-1 Standard specifies the technical delivery conditions for two qualities TR1 and TR2 of seamless tubes of circular cross section with specified room temperature properties made of non-alloy quality steel.

en10216

EN 10216-1 P235 Seamless steel tubes for pressure purposes Quick Details
Manufacture:Seamless process
Out Dimensions: 14mm-509mm
Wall Thickness: 2mm-50mm
Length: Fixed(6m,9m,12,24m) or normal length(5-12m)
Ends: Plain End, Beveled End, Treaded

Manufacturing process
Steels shall be fully killed.
NOTE :This excludes the use of rimming, balanced or semi-killed steel.

The steel name:
(1)the capital letter P for pressure purposes;
(2)the alphanumeric TR1 for qualities without specified aluminium content, impact properties and specific inspection and testing requirements ;
(3)the alphanumeric TR2 for qualities with specified aluminium content, impact properties and specific inspection and testing requirements.

Tube manufacture and delivery conditions
EN 10216-1 P235 Seamless steel tubes will be manufactured by a seamless process. The forming operations and delivery conditions are shown in Table 1.

Table 1 — Forming operations and delivery conditions
Forming operation Quality Delivery condition
Hot formed TR1 As formed or normalized or normalizing-formed

TR2 Normalized or normalizing-formed
Hot formed + cold finished TR1 and TR2 Normalized

Chemical composition of EN 10216-1 P235

Chemical composition (cast analysis) a in % by mass for quality TR2
Steel grade Steel
number
C
max.
Si
max.
Mn
max.
P
max.
S
max.
Cr
max.
Mo
max
P235TR2 1.0255 0,16 0,35 1,20 0,025 0,015 0,30 0,08

 

Ni max. Al tot min. Cu max Nb max. Ti max. V max. Cr+Cu+Mo+Ni max.
0,30 0,02
d
0,30 0,010 0,04 0,02 0,70

Chemical composition (cast analysis) a in % by mass for quality TR1

Steel grade Steel
number
C
max.
Si
max.
Mn
max.
P
max.
S
max.
Cr
b
max.
Mo
b
max
P235TR1 1.0254 0,16 0,35 1,20 0,025 0,020 0,30 0,08

 

Ni max. Al tot min. Cu max Nb max. Ti max. V max. Cr+Cu+Mo+Ni max.
0,30 - 0,30 0,010 0,04 0,02 0,70

Mechanical properties of EN 10216-1 P235

Mechanical properties for quality TR2

Steel grade Tensile properties Impact properties
Steel name Steel
number
Upper yield strength
R eH
b min. for Wall Thickness
T mm
Tensile
Strength
R m
Elongation
A min. %
b
c
Minimum average
absorbed energy
KV 2 J
at a temperature of °C
c
T ≤ 16 16 < T ≤ 40 40 < T ≤
60
l t
MPa * MPa * MPa * MPa * l t 0 -10 0
P235TR2 1.0255 235 225 215 320 to 440 25 23 40 28 d 27

Note: l = longitudinal t = transverse

Mechanical properties for quality TR1

Steel grade Tensile properties Impact properties
Steel name Steel
number
Upper yield strength
R eH
b min. for Wall Thickness
T mm
Tensile
Strength
R m
Elongation
A min. %
b
c
Minimum average
absorbed energy
KV 2 J
at a temperature of °C
c
T ≤ 16 16 < T ≤ 40 40 < T ≤
60
l t
MPa * MPa * MPa * MPa * l t 0 -10 0
P235TR1 1.0254 235 225 215 360 to 550 25 23 - - -

Note: l = longitudinal t = transverse

Tolerances of EN 10216-1 Seamless steel tubes

Tolerances on outside diameter and on wall thickness

Outside
diameter D
mm
Tolerances on D Tolerances on T for a T/D ratio
≤ 0,025 > 0,025
≤ 0,050
> 0,050
≤ 0,10
> 0,10
D ≤ 219,1 ± 1% or ± 0,5 mm whichever is the greater ± 12,5 % or ± 0,4 mm
whichever is the greater
D > 219,1 ± 20 % ± 15 % ± 12,5 % ± 10 % a
a For outside diameters D ≥ 355,6 mm it is permitted to exceed the upper wall thickness locally by a further 5 % of the wall thickness T

Tolerances on exact lengths 

Length L Tolerance on exact length
L ≤ 6 000 + 10
0
6 000 < L ≤ 12 000 +15
0
L > 12 000
+by agreement
0


Contact Us

Telephone:
+86-0731-8867-8530
Address:
Hunan Steel Industrial Zone,No.9 Xiangfu Road, Yuhua District,Changsha,Hunan,China.

Product

Quick Links

Get a Quote
Copyright © Bestar Steel Co., Ltd. All Rights Reserved.