ASTM A500 Rectangular Tube

Views: 0     Author: Site Editor     Publish Time: 2023-10-13      Origin: Site

Inquire

As the name suggests, rectangular tubes are hollow, long steel materials also referred to as flat tubes, flat square tubes, or square flat tubes. In the manufacturing of mechanical parts and engineering structures, it is commonly employed when the torsional and bending strengths are equal because it results in a lighter product.

Published by ASTM International, ASTM A500 is a standard specification for seamless and weldable carbon structural steel. Rectangular steel pipe, ASTM A500, is suitable for general structural applications such as bridges and buildings, and it can be fastened with bolts, rivets, or welding.

ASTM A500 Rectangular tube

Tensile Properties of ASTM A500 Rectangular Tubes

ASTM A500 Rectangular Tube
Minimum stretch(Mpa) 310 400 427 400
Yield Strength (Mpa) 269 317 345 250
Minimum elongation per 50.8mm, %D 25A 13B 21C 23B

Notes
A: Suitable for steel pipes with wall thickness (t) ≥ 3.05mm. For thinner steel pipes, the minimum elongation can be calculated by the following formula: Secondary length per 50.8mm = 56t+17.5, rounded to two decimal places.
B: Suitable for steel pipes with wall thickness (t) ≥ 4.57mm. For thinner steel pipes, the minimum elongation can be calculated by the following formula: Elongation per 50.8mm = 61t+12, rounded to two decimal places.
C: Suitable for steel pipes with wall thickness (t) ≥ 3.05mm. For thinner tubes, the minimum secondary length can be agreed with the manufacturer.
D: The specified minimum elongation is only a reference value for test experiments, not a technical standard for steel pipe trade.


Contact Us

Telephone:
+86-0731-8867-8530
Address:
Hunan Steel Industrial Zone,No.9 Xiangfu Road, Yuhua District,Changsha,Hunan,China.

Product

Quick Links

Get a Quote
Copyright © Bestar Steel Co., Ltd. All Rights Reserved.