ASTM A53 ERW Steel Pipe
Home » News » Company News » ASTM A53 ERW Steel Pipe

ASTM A53 ERW Steel Pipe

Views: 0     Author: Site Editor     Publish Time: 2024-01-10      Origin: Site

Inquire

ASTM A 53 Type E is a standard of ERW (Electric Resistance Welded) pipe material, which can be divided into Grade A and Grade B.

Chemical Requirements of ASTM A53 ERW Steel Pipe

Type E
(electric resistance welded)
Chemical Content Grade A Grade B
Carbon max. % 0.25 0.30*
Manganese max. % 0.95 1.2
Phosphorous max. % 0.05 0.05
Sulfur max. % 0.045 0.045
Copper max. % 0.40 0.40
Nickel max. % 0.40 0.40
Chromium max. % 0.40 0.40
Molybdenum max. % 0.15 0.15
Vanadium max. % 0.08 0.08

* For each reduction below 0.01% below the specified carbon maximum, an increase of 0.06% manganese above the specified maximum will be permitted up to a maximum of 1.65% (does not apply to SA53).

Mechanical Properties Of ASTM A53ERW Steel Pipe

Types and Grades Min. Tensile Strength Min. Yield Strength
Type E Grade A 330Mpa / 48000psi 205Mpa / 30000psi
Type E Grade B 415Mpa / 60000psi 240Mpa / 35000psi

 

Test of ASTM A53 Pipe

- Chemical Analysis

- Tensile Test

- Bending Test

- Flattening Test

- Hydro-Test

- Weld Seam Ultrasonic or Electromagnetic Test


Contact Us

Telephone:
+86-0731-8867-8530
Address:
Hunan Steel Industrial Zone,No.9 Xiangfu Road, Yuhua District,Changsha,Hunan,China.

Product