1. Welded steel pipes for low-pressure fluid transportation (GB/T3092-1993) are also called generally welded pipes, commonly known as clarinet pipes. It is a welded steel pipe used for conveying water, gas, air, oil, heating steam, and other general lower-pressure fluids and other purposes. The wall thickness of the steel pipe is divided into ordinary steel pipe and thickened steel pipe; the form of the pipe end is divided into unthreaded steel pipe (light pipe) and threaded steel pipe. The specification of the steel pipe is expressed by the nominal diameter (mm), and the nominal diameter is an approximate value of the inner diameter. It is customary to express in inches, such as 11/2 and so on. In addition to being directly used to transport fluids, welded steel pipes for low-pressure fluid transportation are also widely used as raw pipes for galvanized welded steel pipes for low-pressure fluid transportation.
2. Galvanized welded steel pipe for low-pressure fluid transportation (GB/T3091-1993) is also called galvanized electric welded steel pipe, commonly known as a white pipe. It is a hot-dip galvanized welded (furnace welded or electrically welded) steel pipe used for conveying water, gas, air oil, heating steam, warm water, and other general lower-pressure fluids or other purposes. The wall thickness of the steel pipe is divided into ordinary galvanized steel pipe and thickened galvanized steel pipe; the form of the pipe end is divided into non-threaded galvanized steel pipe and threaded galvanized steel pipe. The specification of the steel pipe is expressed by the nominal diameter (mm), and the nominal diameter is an approximate value of the inner diameter. It is customary to express in inches, such as 11/2 and so on.
3. Ordinary carbon steel wire casing (GB3640-88) is a steel pipe used to protect wires in electrical installation projects such as industrial and civil buildings, and installation of machinery and equipment.
4. Straight seam electric welded steel pipe (YB242-63) is a steel pipe whose weld seam is parallel to the longitudinal direction of the steel pipe. It is usually divided into metric electric welded steel pipe, electric welded thin-walled pipe, transformer cooling oil pipe, and so on.

High-frequency straight seam steel pipe standard code:
1. Welded steel pipes for low-pressure fluid transportation (GB/T3092-1993) are also called generally welded pipes, commonly known as clarinet pipes. It is a welded steel pipe used for conveying water, gas, air, oil, heating steam, and other general lower-pressure fluids and other purposes. The wall thickness of the steel pipe is divided into ordinary steel pipe and thickened steel pipe; the form of the pipe end is divided into unthreaded steel pipe (light pipe) and threaded steel pipe. The specification of the steel pipe is expressed by the nominal diameter (mm), and the nominal diameter is an approximate value of the inner diameter. It is customary to express in inches, such as 11/2 and so on. In addition to being directly used to transport fluids, welded steel pipes for low-pressure fluid transportation are also widely used as raw pipes for galvanized welded steel pipes for low-pressure fluid transportation.
2. Galvanized welded steel pipe for low-pressure fluid transportation (GB/T3091-1993) is also called galvanized electric welded steel pipe, commonly known as a white pipe. It is a hot-dip galvanized welded (furnace welded or electrically welded) steel pipe used for conveying water, gas, air oil, heating steam, warm water, and other general lower-pressure fluids or other purposes. The wall thickness of the steel pipe is divided into ordinary galvanized steel pipe and thickened galvanized steel pipe; the form of the pipe end is divided into non-threaded galvanized steel pipe and threaded galvanized steel pipe. The specification of the steel pipe is expressed by the nominal diameter (mm), and the nominal diameter is an approximate value of the inner diameter. It is customary to express in inches, such as 11/2 and so on.
3. Ordinary carbon steel wire casing (GB3640-88) is a steel pipe used to protect wires in electrical installation projects such as industrial and civil buildings, and installation of machinery and equipment.
4. Straight seam electric welded steel pipe (YB242-63) is a steel pipe whose weld seam is parallel to the longitudinal direction of the steel pipe. Usually divided into metric electric welded steel pipe, electric welded thin-walled pipe, transformer cooling oil pipe


Contact Us

Telephone:
+86-0731-8867-8530
Address:
Hunan Steel Industrial Zone,No.9 Xiangfu Road, Yuhua District,Changsha,Hunan,China.

Product

Quick Links

Get a Quote
Copyright © Bestar Steel Co., Ltd. All Rights Reserved.