How should the spiral steel pipe be anti-corrosion in the water supply pipe
Home » News » Company News » How should the spiral steel pipe be anti-corrosion in the water supply pipe

How should the spiral steel pipe be anti-corrosion in the water supply pipe

Views: 0     Author: Site Editor     Publish Time: 2022-09-11      Origin: Site

Inquire

Usually, we use epoxy coal tar paint. If the requirements are high, 3 oil and 2 cloth can be used. 3 coats of paint and 2 coats of fiberglass cloth, staggered construction. If it is required, the primer and topcoat of epoxy coal tar can be used directly, and each construction is done twice. Simple and convenient, generally this is the solution.

The interior of the steel pipe depends on whether it is edible water. If it is, use environmentally friendly paint, such as epoxy polyamide paint.

The base material of PE anti-corrosion steel pipe includes seamless steel pipe, spiral steel pipe, and straight seam steel pipe. The three-layer polyethylene (3PE) anti-corrosion coating is widely used in the oil pipeline industry due to its good corrosion resistance, water vapor permeability resistance, and mechanical properties. 3PE anti-corrosion steel pipe 3PE anti-corrosion steel pipe three-layer structure polyethylene anti-corrosion layer (3PE) combines the excellent properties of the two kinds of anti-corrosion layers of fusion-bonded epoxy powder coating and extruded polyethylene, and combines the interface characteristics of fusion-bonded epoxy powder coating with The chemical resistance properties, combined with the mechanical protection properties of the extruded polyethylene coating, lead to a significant improvement in the respective properties. Therefore, it is very advantageous as an outer protective layer for buried pipelines.


Contact Us

Telephone:
+86-0731-8867-8530
Address:
Hunan Steel Industrial Zone,No.9 Xiangfu Road, Yuhua District,Changsha,Hunan,China.

Product

Quick Links

Get a Quote
Copyright © Bestar Steel Co., Ltd. All Rights Reserved.