Steel Pipe Surface Problems And Solutions
Home » News » Company News » Steel Pipe Surface Problems And Solutions

Steel Pipe Surface Problems And Solutions

Views: 0     Author: Site Editor     Publish Time: 2023-12-14      Origin: Site

Inquire

1. Causes and solutions for fish eyes on the outer surface of steel pipes
Possible reasons: The machine head temperature is too high and cooling is insufficient.
Troubleshooting method: lower the machine head temperature and increase the cooling water volume

2. Causes and solutions to the rough surface of steel pipes
Possible reasons: ① The material contains too much moisture; ② The material temperature is low; ③ The die is not clean; ④ The extrusion speed is too fast.
Troubleshooting methods: ① Increase the temperature of the dryer to dry the material; ② Adjust the process temperature; ③ Clean the die; ④ Adjust the extrusion speed.


Contact Us

Telephone:
+86-0731-8867-8530
Address:
Hunan Steel Industrial Zone,No.9 Xiangfu Road, Yuhua District,Changsha,Hunan,China.

Product

Quick Links

Get a Quote
Copyright © Bestar Steel Co., Ltd. All Rights Reserved.