What Is Spiral Welded Pipe?
Home » News » Company News » What Is Spiral Welded Pipe?

What Is Spiral Welded Pipe?

Views: 0     Author: Site Editor     Publish Time: 2023-10-17      Origin: Site

Inquire

What is SSAW Steel Pipe?

SSAW steel pipe(Spiral Submerged arc welding pipe) is made up of hot-rolled coiled steel using a double-sided submerged arc welding method. The welding process allows the steel pipes manufacturers to produce large-diameter steel pipes suitable for different applications.

Short Description:

FOB Price: US $0.5 – 9,999 / Piece
Min.Order Quantity: 100 Piece/Pieces
Supply Ability: 10000 Piece/Pieces per Month
Keywords: SSAW Pipe, SSAW Steel Pipe, Spiral Steel Pipe, Welded Spiral Pipe
Size: OD: 219.1mm ~ 3500mm; WT: 6mm ~ 25mm (Up to 1”);LENGTH: 6mtr ~ 18mtr, SRL, DRL
Standard & Grade: ASTM A53 Grade A/B/C, AWWA C200
Ends: Beveled Ends, Square Cut, With LTC/STC/BTC/VAM Connection
Packing: In Bulk, Ends Protector on Both Sides, Waterproof Materials Wrapped
Usage: Used for low pressure liquid delivery, such as water, gas, and oi

spiral welded pipe

 

Sizes of SSAW Steel Pipe(Spiral Submerged Arc Pipe)

Out diameter:219mm-3620mm

Wall thickness: 5mm-25.4mm

Length: 3m-12m

Chemical Analysis and Mechanical Properties of SSAW Steel Pipe

 

Standard Grade Chemical Composition(max)% Mechanical Properties(min)
C Si Mn P S Tensile Strength(Mpa) Yield Strength(Mpa)
API 5CT h40 - - - - 0.030 417 417
J55 - - - - 0.030 517 517
K55 - - - - 0.300 655 655
API 5L PSL1 A 0.22 - 0.90 0.030 0.030 335 335
B 0.26 - 1.20 0.030 0.030 415 415
X42 0.26 - 1.30 0.030 0.030 415 415
X46 0.26 - 1.40 0.030 0.030 435 435
X52 0.26 - 1.40 0.030 0.030 460 460
X56 0.26 - 1.40 0.030 0.030 490 490
X60 0.26 - 1.40 0.030 0.030 520 520
X65 0.26 - 1.45 0.030 0.030 535 535
X70 0.26 - 1.65 0.030 0.030 570 570
API 5L PSL2 B 0.22 0.45 1.20 0.025 0.015 415 415
X42 0.22 0.45 1.30 0.025 0.015 415 415
X46 0.22 0.45 1.40 0.025 0.015 435 435
X52 0.22 0.45 1.40 0.025 0.015 460 460
X56 0.22 0.45 1.40 0.025 0.015 490 490
X60 0.12 0.45 1.60 0.025 0.015 520 520
X65 0.12 0.45 1.60 0.025 0.015 535 535
X70 0.12 0.45 1.70 0.025 0.015 570 570
X80 0.12 0.45 1.85 0.025 0.015 625 625
ASTM A53 A 0.25 0.10 0.95 0.050 0.045 330 330
B 0.30 0.10 1.20 0.050 0.045 415 415
ASTM A252 1 - - - 0.050 - 345 345
2 - - - 0.050 - 414 414
3 - - - 0.050 - 455 455
EN10217-1 P195TR1 0.13 0.35 0.70 0.025 0.020 320 320
P195TR2 0.13 0.35 0.70 0.025 0.020 320 320
P235TR1 0.16 0.35 1.20 0.025 0.020 360 360
P235TR2 0.16 0.35 1.20 0.025 0.020 360 360
P265TR1 0.20 0.40 1.40 0.025 0.020 410 410
P265TR2 0.20 0.40 1.40 0.025 0.020 410 410
EN10217-2 P195GH 0.13 0.35 0.70 0.025 0.020 320 320
P235GH 0.16 0.35 1.20 0.025 0.020 360 360
P265GH 0.20 0.40 1.40 0.025 0.020 410 410
EN10217-5 P235GH 0.16 0.35 1.20 0.025 0.020 360 360
P265GH 0.20 0.40 1.40 0.025 0.020 410 410
EN10219-1 S235JRH 0.17 - 1.40 0.040 0.040 360 360
S275JOH 0.20 - 1.50 0.035 0.035 410 410
S275J2H 0.20 - 1.50 0.030 0.030 410 410
S355JOH 0.22 0.55 1.60 0.035 0.035 470 470
S355J2H 0.22 0.55 1.60 0.030 0.030 470 470
S355K2H 0.22 0.55 1.60 0.030 0.030 470 470

Standard and Classfication 

Classfication Standard Main Products
Steel Pipe for Fluid Service GB/T 14291 Welded pipe for mine fluid sevice
GB/T 3091 Welded pipe for low pressure fluid service
SY/T 5037 Spirally submerged arc welded steel pipe for pipelines for low pressure fluid service
ASTM A53 Black and hot-hipped galvanized welded and seamless steel pipe
BS EN10217-2 Welded steel tybes for pressure purposes – delivery technical conditions – part2: Electric welded non- alloy and alloy steel tubes with specified elevated temperature properties
BS EN10217-5 Welded steel tybes for pressure purposes – delivery technical conditions – part5: submerged arc welded non-alloy and alloy steel tubes with specified elevated temperature properties
Steel Pipe for Ordinary Structure GB/T 13793 Longitudinally electric resistance welded steel pipe
SY/T 5040 Spirally submerged arc welded steel pipe piles
ASTM A252 Welded and seamless steel pipe piles
BS EN10219-1 Cold formed welded structural hollow sections of non-alloy and fine grain steels – part1: Technical delivert conditions
BS EN10219-2 Cold formed welded structural hollow sections of non-alloy and fine grain steels – part2: tolerances dimmsions and sectional properties
Line Pipe GB/T 9711.1 Steel pipe for pipeline transportation system of petroleum and natural gas industries(Class A steel pipe)
GB/T 9711.2 Steel pipe for pipeline transportation system of petroleum and natural gas industries(Class B steel pipe)
API 5L PSL1/2 Line pipe
Casing API 5CT Steel pipe for use as casing or tubing for wells of petroleum and natural gas industries

The Advantages of SSAW Pipes

SSAW steel pipe can be produced in longer length (maximum length up to 50 meters) compared to LSAW steel pipes

Due to its spiral seam SSAW pipe has an accurate diameter accuracy and strength

The sizes are adjustable & can be tailored to end-users requirement

Usage: Used for low pressure liquid delivery, such as water, gas, and oil.

SSAW steel pipe is the raw material of strip coil, often temperature extrusion molding, automatic double-wire double submerged arc welding process made of spiral seam pipe. Spiral steel pipe will strip into the pipe unit, the multi-roll rolling, strip rolled up, forming a circular gap opening gap, adjust the squeeze roll reduction, the weld gap control in the 1 ~ 3mm, and make both ends of the weld flush.

We have engaged in the steel pipe industry for 30years with rich exprience and strong strengths.  Welcome to contact us to get more information about spiral welded pipe!


Contact Us

Telephone:
+86-0731-8867-8530
Address:
Hunan Steel Industrial Zone,No.9 Xiangfu Road, Yuhua District,Changsha,Hunan,China.

Product