304 Pipe

Short Description:

Type: Stainless Steel 304 Pipe, Stainless Steel 304 Tube, 304 welded pipe, 304 seamless pipe
Spec.: OD: 3-1219mm. WT: SCH 5S, SCH 10S, SCH 40S, SCH 80S. LENGTH: Single/Double Random, Max to 23m.
Standard: ASTM A269, ASTM A312, ASTM A554, ASTM A358, ASTM A778, ASTM A813, JIS G3459
Grade: 304
Surface: Annealed, Pickling, Polished
Packing: Waterproof paper wrapped, Packed in wooden cabins.


Product Detail

Size Chart

Manufacturing Process

Product Tags

Product Descripition

What is 304 Pipe

Stainless Steel 304 Pipe is ideal for all structural applications where greater strength and superior corrosion resistance are required. Stainless Steel 304 Pipe is a metallic pipe made up of austenitic stainless steel that has 18% chromium and 8% nickel in the composition. Bestar Steel is the leading manufacturer and supplier of stainless steel 304 pipes in various types and sizes. 304 pipe is the most versatile and widely used of various stainless steel pipes due to its versatility and high-end durability. Its chemical composition, mechanical properties, weldability, and corrosion/oxidation resistance provide the best all-round performance stainless steel at a relatively low cost. The 304 pipe provides protection from corrosion and pitting, which adds longer life to the product.

Product Specification

What is the specification of 304 pipe

Standard of 304 pipe:
ASTM: ASTM A312,ASTM A376, ASTM A269, ASTM A249, ASTM A403, ASTM A182, ASTM A351
ASME: ASME SA312, ASME SA376
Pressure: SA358, SA269, SA249, SA403, SA182, SA351

Size Range of 304 pipe:
Seamless steel pipe: OD: 3-600mm. WT: 0.5-100mm, Length: 24000mm
Welded steel pipe: OD: 6-1219mm. WT: 0.3-45mm, Length: 18000mm

Chemical Composition

Chemical Composition of ASTM A312 Stainless Steel 304 Pipe

Grade UNS
Designation
Composition
Carbon Manganese Phosphorous Sulfur Silicon Chromium Nickel Molybdenum
TP304 S30400 0.08 2.00 0.045 0.030 1.00 18.0 – 20.00 8.0-11.0 ...
TP304L S30403 0.035 D 2.00 0.045 0.03 1.00 18.0 – 20.00 8.0-113.0 ...
TP304H S30409 0.04 – 0.10 2.00 0.045 0.03 1.00 18.0 – 20.00 8.0-11.0 ...
... S30415 0.04 – 0.06 0.8 0.045 0.03 1.00 –2.00 18.0 – 19.0 9.0-10.0 ...
TP304N S30451 0.08 2.00 0.045 0.03 1.00 18.0 – 20.00 8.0-18.0 ...
TP304LN S30453 0.035 2.00 0.045 0.03 1.00 18.0 – 20.00 8.0-12.0 ...

Mechanical Properties

Mechanical Properties of ASTM A312 Stainless Steel 304 Pipe

Grade UNS
Designation
Tensile Strength
min, ksi [MPa]
Yield Strength,
min, ksi [MPa]
TP304 S30400 75[515] 30[205]
TP304L S30403 70[485] 25[170]
TP304H S30409 75[515] 30[205]
. . . S30415 87[600] 42[290]
TP304N S30451 80[550] 35[240]
TP304LN S30453 75[515] 30[205]

Application

304 pipe application

  • Trailers
  • Heat Exchangers
  • Food processing equipment
  • Kitchen benches, sinks, troughs, equipment and appliances
  • construction materials
  • Threaded fasteners
  • Chemical containers, including for transport
  • Automotive trim
  • Architectural applications
  • Railway cars
  • Woven or welded screens for mining, quarrying & water filtration

  • Previous:
  • Next:

  • Size Chart of Stainless Steel 304 Pipe

    NPS Designator Outside Diameter in. Schedule 5S in. Schedule 10S in. Schedule 40S in. Schedule 80S in.
    1/4 0.54 0.065 0.088 0.119
    3/8 0.675 0.065 0.091 0.126
    1/2 0.84 0.065 0.083 0.109 0.147
    3/4 1.05 0.065 0.083 0.113 0.154
    1.0 1.315 0.065 0.109 0.133 0.179
    1 1/4 1.66 0.065 0.109 0.14 0.191
    1 1/2 1.9 0.065 0.109 0.145 0.2
    2 2.375 0.065 0.109 0.154 0.218
    2 1/2 2.875 0.083 0.12 0.203 0.276
    3 3.5 0.083 0.12 0.216 0.3
    3 1/2 4 0.083 0.12 0.226 0.318
    4 4.5 0.083 0.12 0.237 0.337
    5 5.563 0.109 0.134 0.258 0.375
    6 6.625 0.109 0.134 0.28 0.432
    8 8.625 0.109 0.148 0.322 0.5
    10 10.75 0.134 0.165 0.365 0.5
    12 12.75 0.156 0.18 0.375 0.5

    Manufacturing Process of Stainless Steel 304 Pipe:

    stianless_steel_welded_pipe_manufacturing_process

    stainless_steel_seamless_pipe

    Test:

    PMI test

    PMI test