Carbon Steel ERW Pipe

Short Description:

Type: Carbon Steel ERW Pipe,Electric Resistance Welded Steel Pipe
Spec.: OD: 21.3mm-660mm, WT:1-20mm. or  sch5, sch10, sch40, sch80, st, xs  LENGTH: 5.8mtr ~ 22mtr
Standard: ASTM 5L, ASTM A53, ASTM A178, ASTM A500/501, ASTM A252, ASTM A135, EN 10219, EN10224, JIS G3466 , etc
Grade:
API 5L: PSL1/PSL2  Gr.A, Gr.B, X42, X46, X52, X56, X60, X65, X70
ASTM A53: GR.A, GR.B,
EN: S275, S275JR, S355JRH, S355J2H
GB: Q195, Q215, Q235, Q345, L175, L210, L245, L320, L360-L555
Ends: Square Ends/Plain Ends (straight cut, saw cut, torch cut), Beveled/Threaded Ends
Coating: Zinc/Anti-corrosive Coating
Packing: Bundled/In Bulk, Plastic Caps Plugged, Waterproof Paper Wrapped

Note: Other grades of steel pipe can be made available through consultations.


Product Detail

Manufacturing Process

Application

Product Tags

Details of Carbon Steel ERW Pipe

What is the Carbon Steel ERW Pipe?

Carbon Steel ERW Pipe is a versatile, economical, and efficient pipe made by using electrical resistance to forge-weld the edges of a formed steel strip. Modern HFI-ERW technology produces a high-integrity weld, making these pipes the go-to choice for a vast range of small to medium-diameter applications in energy, construction, and industry, effectively bridging the gap between seamless and large-diameter welded pipes.

Product Specification and Size of Carbon Steel ERW Pipe

Available Specification of Carbon Steel ERW Pipe

Standard

ASTM 5L, ASTM A53, ASTM A178, ASTM A500/501, ASTM A252, ASTM A135, EN 10219, EN10224, JIS G3466 , etc

                                   Material

L245/B L290/X42 L320/X46L360/X52 L415/X60Q355

                          Outside Diameter

Minimum (Φ21.3mm ) O.D    Maximum  (Φ 660mm) O.D

Wall Thickness

Minimum 1mm   Maximum 20mm

                              Pipe Length

Minimum:5.8m  Maximum : 22m

 

 

 

 

 Products Specifications

 

 

 

 

 

 

 

 

 

 

Φ88.9mmx2.11mm-10mm Φ355.6mmx 5.0mm-14mm
Φ101.6mmx2.11mm-10mm Φ377mmx5.0mm-14mm
Φ108mmx2.11mm-10mm Φ406.4mmx5.0mm-14mm
Φ114.3mmx 2.11mm-l1.13mm Φ426mmx5.0mm-14mm
Φ141.3mm×2.77mm-11.13mm Φ457.2mmx6.0mm-22mm
Φ159mmx2.5mm-11.13mm Φ508mmx6.0mm-22mm
Φ168mmx2.77mm-11.13mm Φ529mmx6.0mm-22mm
Φ219.1mmx2.77mm-12.7mm Φ559mmx6.0mm-22mm
Φ245mmx5.0mm-14mm Φ610mmx6.0mm-22mm
Φ273.1mmx 5.0mm-14mm Φ630mmx6.0mm-22mm
Φ323.9mmx5.0mm-14mm Φ660mmx6.0mm-22mm

Chemical Composition of Carbon Steel ERW Pipe

Chemical Analysis and Mechanical Properties of ERW Steel Pipe

Chemical Analysis and Mechanical Properties

Standard Class Grade

Chemical Analysis(%)

Mechanical Properties(min)(Mpa)

C

Mn

P

S

Tensile Strength Yield Strength
API 5L PSL1

B

0.26

1.2

0.03

0.03

414

241

X42

0.26

1.3

0.03

0.03

414

290

X46

0.26

1.4

0.03

0.03

434

317

X52

0.26

1.4

0.03

0.03

455

359

X56

0.26

1.4

0.03

0.03

490

386

X60

0.26

1.4

0.03

0.03

517

414

X65

0.26

1.45

0.03

0.03

531

448

X70

0.26

1.65

0.03

0.03

565

483

PSL2

B

0.22

1.2

0.025

0.015

414

241

X42

0.22

1.3

0.025

0.015

414

290

X46

0.22

1.4

0.025

0.015

434

317

X52

0.22

1.4

0.025

0.015

455

359

X56

0.22

1.4

0.025

0.015

490

386

X60

0.22

1.4

0.025

0.015

517

414

X65

0.22

1.45

0.025

0.015

531

448

X70

0.22

1.65

0.025

0.015

565

483

X80

0.22

1.85

0.025

0.015

621

552


  • Previous:
  • Next:

  • Manufacturing Process of Carbon Steel ERW Pipe

     

    Application of Carbon Steel ERW Pipe

    Due to their cost-effectiveness and reliability in medium-pressure applications, Carbon Steel ERW pipes are ubiquitous:

    • Oil and Gas Gathering Lines: Transporting hydrocarbons from the wellhead to processing facilities.
    • Fuel and Water Pipelines: In refineries, chemical plants, and municipal water systems.
    • Structural Applications: As scaffolding, fencing, street lighting poles, and in construction frameworks.
    • Automotive and Mechanical Parts: As structural components and sleeves.
    • API Line Pipe: Many are manufactured to API 5L standards for use in the energy industry.