Carbon Steel SSAW Pipe

Short Description:

Type: Carbon Steel SSAW Pipe,Spiral Submerged Arc Welded Pipe
Spec.: OD: 219mm-3000mm, WT:6-25mm. LENGTH: 6mtr ~ 18mtr
Standard: API 5L PSL1/PSL2 Gr.A, Gr.B, X42, X46, X52, X56, X60, X65, X70;  ASTM A53/A252/A500; EN10219/EN10208/EN10297, JIS G3457
Coating Standard: ANSI/AWWA C104/A21.4 American National Standard for Cement-Mortar Lining for ductile-iron Pipe and Fittings for water
DIN 30670 Polyethylene coatings of steel and fittings.
Grade: Q235A, Q235B, Q345, L245(B), L290 (X42), L320 (X46), L360 (X52), L390(X56), L415(X60), L450(X65), L485(X70), L555(X80),
L290M (X42M), L360M (X52M), L390M(X56M), L415M(X60M), L450M(X65M), L485M(X70M), L555M(X80M).
Ends: Square Ends/Plain Ends (straight cut, saw cut, torch cut), Beveled/Threaded Ends
Coating: Zinc/Anti-corrosive Coating
Packing: Bundled/In Bulk, Plastic Caps Plugged, Waterproof Paper Wrapped


Product Detail

Manufacturing Process

Application

Product Tags

Details of Carbon Steel SSAW Pipe

What is the Carbon Steel SSAW Pipe?

Carbon Steel SSAW Pipe is a large-diameter, spirally welded pipe known for its production flexibility and cost-effectiveness for a wide range of diameters. While it shares the high-quality submerged arc weld with LSAW pipe, its helical seam makes it ideally suited for structural applications like piling and for fluid transmission in projects where the ultimate high-pressure capability of a longitudinal seam is not the primary requirement.

Product Specification and Size of Carbon Steel SSAW Pipe

Available Specification of Carbon Steel SSAW Pipe

Chemical Composition of Carbon Steel SSAW Pipe

Chemical Analysis and Mechanical Properties of SSAW Steel Pipe

Standard Grade Chemical Composition(max)% Mechanical Properties(min)
C Si Mn P S Tensile Strength(Mpa) Yield Strength(Mpa)
API 5CT h40 - - - - 0.030 417 417
J55 - - - - 0.030 517 517
K55 - - - - 0.300 655 655
API 5L PSL1 A 0.22 - 0.90 0.030 0.030 335 335
B 0.26 - 1.20 0.030 0.030 415 415
X42 0.26 - 1.30 0.030 0.030 415 415
X46 0.26 - 1.40 0.030 0.030 435 435
X52 0.26 - 1.40 0.030 0.030 460 460
X56 0.26 - 1.40 0.030 0.030 490 490
X60 0.26 - 1.40 0.030 0.030 520 520
X65 0.26 - 1.45 0.030 0.030 535 535
X70 0.26 - 1.65 0.030 0.030 570 570
API 5L PSL2 B 0.22 0.45 1.20 0.025 0.015 415 415
X42 0.22 0.45 1.30 0.025 0.015 415 415
X46 0.22 0.45 1.40 0.025 0.015 435 435
X52 0.22 0.45 1.40 0.025 0.015 460 460
X56 0.22 0.45 1.40 0.025 0.015 490 490
X60 0.12 0.45 1.60 0.025 0.015 520 520
X65 0.12 0.45 1.60 0.025 0.015 535 535
X70 0.12 0.45 1.70 0.025 0.015 570 570
X80 0.12 0.45 1.85 0.025 0.015 625 625
ASTM A53 A 0.25 0.10 0.95 0.050 0.045 330 330
B 0.30 0.10 1.20 0.050 0.045 415 415
ASTM A252 1 - - - 0.050 - 345 345
2 - - - 0.050 - 414 414
3 - - - 0.050 - 455 455
EN10217-1 P195TR1 0.13 0.35 0.70 0.025 0.020 320 320
P195TR2 0.13 0.35 0.70 0.025 0.020 320 320
P235TR1 0.16 0.35 1.20 0.025 0.020 360 360
P235TR2 0.16 0.35 1.20 0.025 0.020 360 360
P265TR1 0.20 0.40 1.40 0.025 0.020 410 410
P265TR2 0.20 0.40 1.40 0.025 0.020 410 410
EN10217-2 P195GH 0.13 0.35 0.70 0.025 0.020 320 320
P235GH 0.16 0.35 1.20 0.025 0.020 360 360
P265GH 0.20 0.40 1.40 0.025 0.020 410 410
EN10217-5 P235GH 0.16 0.35 1.20 0.025 0.020 360 360
P265GH 0.20 0.40 1.40 0.025 0.020 410 410
EN10219-1 S235JRH 0.17 - 1.40 0.040 0.040 360 360
S275JOH 0.20 - 1.50 0.035 0.035 410 410
S275J2H 0.20 - 1.50 0.030 0.030 410 410
S355JOH 0.22 0.55 1.60 0.035 0.035 470 470
S355J2H 0.22 0.55 1.60 0.030 0.030 470 470
S355K2H 0.22 0.55 1.60 0.030 0.030 470 470

  • Previous:
  • Next:

  • Manufacturing Process of Carbon Steel Welded Pipe

     

    carbon_steel_welded_pipe_manufacturing_process1

    carbon_steel_welded_pipe_manufacturing_process2

    Application of Carbon Steel SSAW Pipe

    Carbon Steel SSAW Pipes are well-suited for:

    • Foundation Piling: Very commonly used as permanent or temporary piles for construction due to their strength and the spiral seam can provide good grip in soil.
    • Water Transmission: For municipal water supply and drainage projects.
    • Structural Supports: Used as columns, poles, and in structural frameworks.
    • Slurry and Dredging Lines: For transporting abrasive materials.
    • Lower-Pressure Oil and Gas Pipelines: Particularly in less critical or gathering lines.