ASTM A53/A795/A135 ERW steel pipe

ASTM A53/A795/A135 ERW steel pipe Featured Image
Loading...
  • ASTM A53/A795/A135 ERW steel pipe
  • ASTM A53/A795/A135 ERW steel pipe
  • ASTM A53/A795/A135 ERW steel pipe
  • ASTM A53/A795/A135 ERW steel pipe

Short Description:

Out Diameter:1/2″-24″

Wall Thickness: 1.65-20mm

Length : 3-12m, or according to customer’s requirement

End : Plain End, Beveled End, Threaded


Product Detail

Product Tags

Bestar Steel’s ERW is available in all the common sizes, up to 24 inch, and is suitable for welding, grooving, threading and bending.

Sizes: 

Out Diameter:1/2"-24"

Wall Thickness: 1.65-20mm

Length : 3-12m, or according to customer’s requirement

End : Plain End, Beveled End, Threaded

 

Standard:

ASTM 5L, ASTM A53, ASTM A178, ASTM A500/501, ASTM A691, ASTM A252, ASTM A672, EN 10217

Steel Grade:

API 5L: PSL1/PSL2  Gr.A, Gr.B, X42, X46, X52, X56, X60, X65, X70

ASTM A53: GR.A, GR.B

EN: S275, S275JR, S355JRH, S355J2H

GB: Q195, Q215, Q235, Q345, L175, L210, L245, L320, L360-L555

 

Uses:

For ERW Line Pipe

For ERW Casing

For ERW Structure Tube

For High pressure and high temperature

 

Surface: Lightly oiled, Hot dip galvanized, Electro galvanized, Black, Bare, Varnish coating/Anti rust oil, Protective Coatings (Coal Tar Epoxy,  Fusion Bond Epoxy, 3-layers PE)

Packing: Plastic plugs in both ends, Hexagonal bundles of max. 2,000kg with several steel strips, Two tags on each bundle, Wrapped in waterproof paper, PVC sleeve, and sackcloth with several steel strips, Plastic caps.

Test: Chemical Component Analysis, Mechanical Properties (Ultimate tensile strength, Yield strength, Elongation), Technical Properties (Flattening Test, Bending Test,  Hardness Test, Impact Test), Exterior Size Inspection, Hydrostatic Test, NDT TEST ( ET TEST, RT TEST, UT TEST)

 

Small diameter erw steel pipe

Out diameter

Sch 5

Sch 10

Sch 40

Inch mm Thickness Kg/mtr Thickness Kg/mtr Thickness Kg/mtr
1/2" 21.3 1.65 0.81 2.11 1.01 2.77 1.29
3/4" 26.7 1.65 1.03 2.11 1.30 2.87 1.71
1" 33.4 1.65 1.31 2.77 2.12 3.38 2.54
1 1/4" 42.2 1.65 1.93 2.77 3.15 3.68 4.11
1 1/2" 48.3 1.65 1.93 2.77 3.15 3.68 4.11
2" 60.3 1.65 2.42 2.77 3.98 4.81 5.31
3" 88.9 2.11 4.58 3.05 6.54 5.49 11.45
3 1/2" 101.6 2.11 5.25 3.05 7.52 5.74 13.77
4" 114.3 2.11 5.25 3.05 7.52 5.74 13.77
5" 141.3 2.77 9.50 3.40 11.74 6.55 22.10
6" 168.3 2.77 11.47 3.40 14.04 7.11 28.68
8" 219.1 2.77 14.99 3.76 20.25 8.18 43.16