News
-
The difference between galvanized steel pipe and plastic coated steel pipe
1. Galvanized steel pipe to make the molten metal react with the iron matrix to produce an alloy layer so that the matrix and the coating are combined. Hot-dip galvanizing is to pickle the steel pipe first. To remove the iron oxide on the surface of the steel pipe, after pickling, it is cleaned b...Read more -
Derusting method and production process of large diameter straight seam steel pipe
Large-diameter straight seam welded pipe is a general name, which is produced by steel strips, and the pipes welded by high-frequency welding equipment are called straight seam welded pipes. (It gets its name because the welding of the steel pipe is in a straight line). Among them, according to d...Read more -
Straight seam steel pipe acceptance method and problem-solving
Acceptance of straight seam steel pipe: 1. The inspection and acceptance of straight seam steel pipes shall be carried out by the technical supervision department of the supplier. 2. The supplier guarantees that the delivery of straight seam steel pipes complies with the provisions of the corresp...Read more -
What is the difference between straight seam steel pipe and seamless steel pipe
A. Different categories 1. Straight seam steel pipe: divided into metric electric welded steel pipe, electric welded thin-walled pipe, transformer cooling oil pipe 2. Seamless steel pipes: seamless pipes are divided into hot-rolled pipes, cold-rolled pipes, cold-drawn pipes, extruded pipes, jacki...Read more -
Causes of problems caused by improper heat treatment of seamless steel pipes
Improper heat treatment of seamless steel pipes is likely to cause a series of production problems, resulting in greatly reduced product quality and turning into waste products. Avoiding mistakes that are easy to make during heat treatment is saving money. What problems should we pay attention to...Read more -
How to carry out anti-corrosion treatment of spiral steel pipe for water delivery
If the spiral steel pipe for water transportation is used to transport tap water or drinking water, the inner wall is usually made of IPN8710 non-toxic anti-corrosion coating, and the outer wall is made of epoxy coal tar pitch for anti-corrosion. Of course, it can also be used for inner and outer...Read more