News
-
Six processing methods of stainless steel pipe fittings
Stainless steel pipe fittings are a kind of pipe fittings. They are made of stainless steel, so they are called stainless steel pipe fittings. They include stainless steel elbows, stainless steel tees, stainless steel crosses, stainless steel reducers, stainless steel pipe caps, etc. It can be di...Read more -
Factors Affecting the Accuracy and Resolution of Wall Thickness Detection of Petroleum Casing
The API standard stipulates that the inner and outer surfaces of the import and export petroleum casing shall not have folds, separations, cracks, and scars. These defects should be completely removed, and the removal depth should not be less than 12.5% of the nominal wall thickness. Oil casing...Read more -
Galvanized steel pipe installation steps
1. Broken pipe: According to the on-site survey and mapping sketch, draw a line on the selected pipe, and break the pipe according to the line. a. To cut the pipe with a grinding wheel, place the pipe on the caliper of the grinding wheel saw, align it with the drawn line, and then cut the pipe. W...Read more -
The purpose of preheating the pipe before welding the spiral steel pipe
Important components of alloy steel and thick parts must be preheated before welding. The purpose of preheating before welding is as follows: (1) Preheating can slow down the cooling rate after welding so that hydrogen diffuses in the weld metal and escapes to avoid cracking caused by hydrogen. I...Read more -
What are the quality requirements for steel pipeline pickling
(1) After pickling, the rust and oil on the inner wall of the steel pipe are completely removed, and the cleanliness should meet the requirements of relevant standards. (2) Pickling parts shall not be over-pickled. If the steel pipe is soaked in the pickling solution for too long, the surface of ...Read more -
The difference between hot-rolled seamless steel pipe and cold-rolled seamless steel pipe
In terms of processing technology: hot rolling is hot working, and cold drawing is cold working. Hot rolling is rolling above the recrystallization temperature, and cold rolling is rolling below the recrystallization temperature; Distinguish from appearance: cold-rolled seamless steel pipe has a ...Read more