Crack types and preventive measures when welding steel pipes
Under the combined effect of welding stress and other embrittlement factors, the metal atomic bonding force in the local area of the welded steel pipe joint is destroyed and the gap formed by the new interface is called welding crack. It has sharp notches and large aspect ratio characteristics....Read more -
Transition Liquid Phase Diffusion Welding of Oil Drill Pipe
Oil drill pipe is made by connecting the drill pipe joint and the rod body after they are manufactured separately. Although friction welding technology has been successfully applied to drill pipe welding, there are still some defects in the actual welding process, such as welding dislocation, fla...Read more -
Structural stainless steel pipes are a light and sturdy choice for industrial projects
Stainless steel pipes are a common and important building material. They are widely used in bridges, building structures, interior decoration, and other fields. In construction projects, structural stainless steel pipes, with their unique properties, give buildings light and sturdy characteristic...Read more -
Performance, application, and market prospects of the industrial DN150 galvanized steel pipe
First, introduction to DN150 galvanized steel pipe DN150 galvanized steel pipe is a steel pipe with an outer diameter of 150mm and an inner diameter of 127mm, mainly used to transport fluids such as water, gas, and air. A galvanized steel pipe is a steel pipe that has been hot-dip galvanized and ...Read more -
Mechanical properties of the industrial Q235 steel pipe compressive strength
First, what is a Q235 steel pipe? Q235 steel pipe is a common carbon structural steel pipe, widely used in construction, bridges, machinery manufacturing, and other fields. It has good plasticity and welding performance, and the price is relatively low, so it has been widely used in engineering. ...Read more -
Plastic coated seamless steel pipe is a high-quality anti-corrosion material
Plastic coated seamless steel pipe is a steel pipe with excellent anti-corrosion performance. On the basis of steel pipe production, a layer of plastic is coated on the surface of the steel pipe through a special process. This special plastic coating process gives the steel pipe excellent anti-co...Read more