Products News

  • Reasons for uneven anti-corrosion thickness of 3PE anti-corrosion steel pipes

    Reasons for uneven anti-corrosion thickness of 3PE anti-corrosion steel pipes

    The industry standard SY/T0413-2002 does not stipulate the uniformity of thickness. It stipulates the low thickness value of the coating but requires that the low thickness value of the coating cannot be lower than the thickness value of the low point, rather than the thickness value of multiple ...
    Read more
  • Heat Treatment of LSAW Steel Pipe

    Heat Treatment of LSAW Steel Pipe

    LSAW steel pipes are frequently used in industry. Heat treatment is a crucial step in their manufacturing process to improve their mechanical properties and ensure proper performance. The heat treatment processes for LSAW steel pipes include normalization, stress relief, quenching, and tempering....
    Read more
  • Characteristics and scope of application of thin-walled stainless steel pipe socket argon arc welding construction method

    Characteristics and scope of application of thin-walled stainless steel pipe socket argon arc welding construction method

    The construction method of thin-walled stainless steel pipe socket argon arc welding has the following characteristics: 1. The welding process does not require welding materials (replaced by expanded pipe edges). The steel pipe is inserted into the pipe fitting socket, and the end of the socket i...
    Read more
  • CS Seamless Pipe Cold Treatment Process

    CS Seamless Pipe Cold Treatment Process

    The production of carbon steel seamless pipes typically involves the use of a cold treatment process to enhance the material’s strength and hardness. Below is an overview of the general cold treatment process for CS seamless pipes. Water Quenching: Water quenching is a common method used in...
    Read more
  • What Is The Difference Between Drill Pipe And Drill Collar?

    What Is The Difference Between Drill Pipe And Drill Collar?

    Both of drill pipe and drill collar are significant oilfield tubular goods. But what is the difference between drill pipe and drill collar? Continue reading to learn more. Drill Pipe: A drill pipe is a long hollow steel tube used to rotate the drill bit and circulate drilling fluid in the well. I...
    Read more
  • Causes of trachoma in welds of spiral submerged arc welded steel pipes

    Causes of trachoma in welds of spiral submerged arc welded steel pipes

    Spiral steel pipe is made of strip steel that is bent in a spiral direction through a rolling machine and then welded by capacitor double-sided submerged arc welding. During the welding production process of spiral steel pipes, many galvanized channel steel problems such as missed welds and misal...
    Read more