Products News
-
Analysis of factors affecting the process of high-frequency straight seam welded pipes
The main process parameters of high-frequency straight seam welded pipes include welding heat input, welding pressure, welding speed, opening angle size, the position and size of the induction coil, the position of the resistor, etc. These parameters have a great impact on improving the quality o...Read more -
Differences and uses of seamless steel pipes and spiral welded pipes
1. Seamless steel pipes are widely used. General-purpose seamless steel pipes are rolled from ordinary carbon structural steel, low alloy structural steel, or alloy structural steel. They have the largest output and are mainly used as pipes or structural parts for transporting fluids. 2. They are...Read more -
How many uses are there for stainless steel pipe fittings
Stainless steel pipe is a kind of hollow round steel, that is mainly widely used in industrial transportation pipelines and mechanical structural components such as petroleum, chemical industry, medical treatment, food, light industry, mechanical instrumentation, etc. In addition, when the bendin...Read more -
Methods for cleaning steel pipes in natural gas pipelines that transport oil, gas, and water together
In the long-term use of natural gas steel pipelines, liquid accumulation in the pipeline and corrosion of the inner wall will occur during the long-term operation of the two-phase flow pipeline. These liquids accumulate at the low points of the pipeline, causing the pressure drop of the pipeline ...Read more -
How to distinguish welded steel pipes and seamless steel pipes
1. Metallographic method: The metallographic method is the main method to distinguish welded steel pipes and seamless steel pipes. High-frequency resistance welded steel pipes do not add welding materials, so the weld seam in the welded steel pipe is very narrow. If the method of rough grinding a...Read more -
Commonly used cold-working forming methods for stainless steel
(1) Cold bending: Cold bending is widely used to make parts from stainless steel sheets and strips. Punch presses are open single-acting, mechanically or hydraulically driven, with a long and narrow workbench. This machine can only produce straight parts, but skilled tool designers can also use i...Read more