Alloy Steel Seamless Pipe
Details of Alloy Steel Seamless Pipe
What is an alloy steel seamless pipe?
There are two types of alloy steel pipe, high alloy steel pipe and low alloy steel pipe. Low alloy steel pipe manufacturing up of pipes with an alloying percentage of less than 5%. A high alloy steel's alloying content would be anything from 5% to roughly 50%. In alloy steel pipe, alloy steel seamless pipe become more and more popular. An alloy steel seamless pipe's working pressure capability is higher than other steel pipes. Alloy Steel Seamless Pipes are utilized in applications that demand moderate corrosion resistance, as well as good durability and a low cost. The High-Temperature Alloy Steel Boiler Pipe is typically utilized in applications where the ambient temperature reaches 500°C.
Chemical Composition of Alloy Steel Seamless Pipe
| C | Mn | P | S | Si | Cr | Mo | V | Nb | B | N | Al | W |
| 0.04-1 | 0.1-0.6 | ≤0.03 | ≤0.01 | 0.5 | 1.9-2.6 | 0.05-0.3 | 0.2-0.3 | 0.02-0.08 | 0.0005-0.006 | ≤0.03 | ≤0.03 | 1.45-1.75 |
Mechanical Property of Alloy Steel Seamless Pipe
| Mechanical Property of Alloy Steel Seamless Pipe | ||
| Tensile Strength (MPa) | Yield Strength (MPa) | Elongation (%) |
| ≥510 | ≥400 | ≥20 |
Equivalent Grades of ASTM A335M Alloy Steel Seamless Pipe
| Name | Temper | Specification | |
| Alloy 4130 | N | MILT6736, AMS6360, AMS6371 | |
| Alloy 4140 | N,A, T | AMS6381 | |
| Alloy 15CDV6 | T1080, T980 | AIR9160C, 1.7734.5, 1.7734.6 | |
| Material and types | Standard Code | Grades includes |
| Alloy Steel Seamless Ferritic and Austentic Boiler, Superheater, IBR approved Heat-Exchanger Pipes | ASTM A213/ ASME SA 213 | T1, T2, T5 , T9, T22, T23, T91, T92 |
| High Temperature Alloy Steel Seamless Pipe (Ferritic) | ASTM A335/ ASME SA 335 | P1, P5, P9, P11, P12, P17, P22, P91, P92 |
| Carbon and Alloy Steel Seamless Mechanical Tubing | ASTM A519/ ASME SA 519 | 4130, 4130X, 4140 |
| High Temperature Alloy Steel Seamless Pipe (Ferritic) | EN10216-2 | 13CrMo4-5 10CrMo9-10 X10CrMoVNb9-1 15NiCuMoNb5-6-4 |
Product Specification and Size of ASTM A335 Alloy Steel Seamless Pipe
Available Specification
| ASTM /ASME | |||
| Product Name | Executive Standard | Dimension (mm) | Steel Code / Steel Grade |
| Seamless Ferritic and Austentic Alloy Steel Boiler, Superheater and Heat-Exchanger Tubes | ASTM A213 | Ø10.3~426 x WT1.0~36 | T5, T9, T11, T12, T22, T91 |
| Seamless Ferritic Alloy Steel Pipes for High Temperature Use | ASTM A335 | Ø1/4"~42" x WT2~120mm | P5, P9, P11, P12, P22, P91, P92 |
| Seamless Carbon and Alloy Steel for Mechanical Tubing | ASTM A519 | Ø16"~42" x WT10~100mm | 4130, 4130X, 4140 |
| EN | |||
| Product Name | Executive Standard | Dimension (mm) | Steel Code / Steel Grade |
| Seamless Ferritic Alloy Steel Pipes for High Temperature Use | EN10216-2 | Ø8"~42" x WT15~100 | 13CrMo4-5, 1-CrMo9-10, X10CrMoVNb9-1, 15NiCuMoNb5-6-4 |
Size Chart of Alloy Steel Seamless Pipe
| Hot Rolled Alloy Steel Seamless Pipe |
Outside Diameter (mm) | Tolerance (mm) |
| OD≤101.6 | +0.4/-0.8 | |
| 101.6<OD≤190.5 | +0.4/-1.2 | |
| 190.5<OD≤228.6 | +0.4/-1.6 | |
| Cold Drawn Alloy Steel Seamless Pipe |
OD<25.4 | ±0.10 |
| 25.4≤OD≤38.1 | ±0.15 | |
| 38.1<OD<50.8 | ±0.20 | |
| 50.8≤OD<63.5 | ±0.25 | |
| 63.5≤OD<76.2 | ±0.30 | |
| 76.2≤OD≤101.6 | ±0.38 | |
| 101.6<OD≤190.5 | +0.38/-0.64 | |
| 190.5<OD≤228.6 | +0.38/-1.14 | |
| NPS Alloy Steel Seamless Pipe |
1/8≤OD≤1-1/2 | ±0.40 |
| 1-1/2<OD≤4 | ±0.79 | |
| 4<OD≤8 | +1.59/-0.79 | |
| 8<OD≤12 | +2.38/-0.79 | |
| OD>12 | ±1% |
Application of Alloy Steel Seamless Pipe
Alloy steel seamless pipe is ideally suitable for chemical, petrochemicals and other energy-related applications. It has characteristics of high corrosion resistance and can be used in a wide range of industrial sectors.
- Off-Shore Oil Drilling Companies
- Power Generation
- Petrochemicals
- Gas Processing
- Specialty Chemicals
- Pharmaceuticals
- Pharmaceutical Equipment
- Chemical Equipment
- Sea Water Equipment
- Heat Exchangers
- Condensers
- Pulp and Paper Industry
- Chemical industries
- Petrochemical industries
- Energy-related applications