Performance characteristics of IPN8710 anti-corrosion steel pipe

The effect of IPN8710 drinking water anti-corrosion steel pipe on tap water and drinking water.

① Modification of epoxy resin. Epoxy resin is a resin with a large number of applications, a wide range, and a very important role so far. However, the major limitations of epoxy resin applied to the inner wall of heavy IPN8710 drinking water pipes are poor weather resistance, easy chalking, high brittleness, and easy discoloration, It is not suitable to be processed into the inner wall of heavy IPN8710 drinking water pipes resistant to chemical atmosphere.

② Modification of the handle enoic acid resin. Mangolic acid resin is a synthetic resin with high decorative and excellent protective properties. Its main advantages are good outdoor weather resistance, excellent adhesion, good alkali resistance, excellent gloss and color retention, good UV resistance, and moisture resistance. , anti-salt spray, anti-mold, good heat resistance and chemical corrosion resistance, bright and full color, hard and wear-resistant, good water and oil resistance, but there are poor ammonia resistance, and unsatisfactory resistance to oxidative acids, acetic acid, and ethanol.

③ Modification of chlorine-containing rubber. Chlorine-containing rubber refers to a rubber polymer containing a large number of chlorine atoms. Its advantages are flame retardant and self-extinguishing, mildew proof, water resistance, acid resistance, alkali resistance, salt resistance, excellent chemical corrosion resistance, good mechanical strength, and easy construction. Restricted by seasons and climatic conditions, the drying speed is fast, and it can form a film at low temperatures, but there are thin anti-corrosion pipeline coatings, high-temperature resistance (generally not exceeding 60°C), poor permeability resistance, solvent resistance, and moisture resistance. Not good, it is difficult to make defects such as the inner wall of the drinking water pipe with high solid weight IPN8710.

④ Modification of other resins. We made use of the advantages of chlorosulfonated polyethylene rubber to modify various resins such as alginic acid resin, alkyd resin, and phenolic resin, and formed the inner wall of BSD series heavy IPN8710 drinking water pipes of BSD brand, so that BSD can stand in the fierce market Set yourself apart from the competition.


Post time: Apr-24-2023