  • Introduction to methods of rust removal from spiral steel pipes

    Introduction to methods of rust removal from spiral steel pipes

    1. Sandblasting and rust removal method: Sandblasting and rust removal uses a high-power motor to drive the sandblasting blades to rotate at high speed so that abrasives such as steel sand, steel shots, iron wire segments, and minerals can sandblast the surface of the steel pipe under the effect ...
    Read more
  • Why stainless steel pipes need solution annealing treatment

    Why stainless steel pipes need solution annealing treatment

    Austenitic stainless steel is softened by solid solution treatment. Generally, the stainless steel pipe is heated to about 950 to 1150°C, and kept for some time, so that the carbides and various alloying elements are fully and evenly dissolved in the austenite, and then quickly quenched to cool. ...
    Read more
  • Basic knowledge of welded steel pipes

    Basic knowledge of welded steel pipes

    Welded steel pipe, also called welded pipe, is a steel pipe made of steel plates or steel strips that are welded after being curled and formed. The production process of welded steel pipes is simple, the production efficiency is high, there are many varieties and specifications, and the equipment...
    Read more
  • The role of steel flange

    The role of steel flange

    Flange, also called flange or flange. It is the part that connects pipes. Connect to the pipe end. There are holes in the flange, and bolts can be inserted to tightly connect the two flanges. The flanges are sealed with gaskets. Flange pipe fittings refer to pipe fittings with flanges (flanges or...
    Read more
  • Why are large-diameter steel pipes mostly welded with steel

    Why are large-diameter steel pipes mostly welded with steel

    1. The uses of large-diameter stainless steel pipes can be divided into oil well pipes (casing, oil pipes, drill pipes, etc.), pipeline pipes, boiler pipes, mechanical structural pipes, hydraulic support pipes, gas cylinder pipes, geological pipes, and chemical pipes (high-pressure fertilizers). ...
    Read more
  • Various connection methods for stainless steel pipes

    Various connection methods for stainless steel pipes

    There are various connection methods for stainless steel pipes. Common pipe fitting types include compression type, compression type, union type, push type, push thread type, socket welding type, union flange connection, welding type and welding and traditional connection. They combined derived s...
    Read more