Products

  • Duplex Steel Seamless Pipe

    Duplex Steel Seamless Pipe

    Type: Duplex Steel Seamless Pipe, Duplex Steel Seamless Tube
    Spec.: Outer Diameter: up to 12″ NB. Thickness: SCH XSS
    Standard: ASTM A790, ASTM A789
    Grade: S31803, S32205, S32750, S32760
    Surface: Annealed, Pickling, Polished
    Packing: Waterproof paper wrapped, Packed in wooden cabins.

  • 304 Pipe

    304 Pipe

    Type: Stainless Steel 304 Pipe, Stainless Steel 304 Tube, 304 welded pipe, 304 seamless pipe
    Spec.: OD: 3-1219mm. WT: SCH 5S, SCH 10S, SCH 40S, SCH 80S. LENGTH: Single/Double Random, Max to 23m.
    Standard: ASTM A269, ASTM A312, ASTM A554, ASTM A358, ASTM A778, ASTM A813, JIS G3459
    Grade: 304
    Surface: Annealed, Pickling, Polished
    Packing: Waterproof paper wrapped, Packed in wooden cabins.

  • 316 Pipe

    316 Pipe

    Type: Stainless Steel 316 Pipe, Stainless Steel 316 Tube, 316 welded pipe, 316 seamless pipe
    Spec.: OD: 3-1219mm. WT: SCH 5S, SCH 10S, SCH 40S, SCH 80S. LENGTH: Single/Double Random, Max to 23m.
    Standard: ASTM A312, ASTM A213, ASTM A269, ASTM A632, ASME SA213, NFA 49-117, BS 10216
    Grade: 316
    Surface: Annealed, Pickling, Polished
    Packing: Waterproof paper wrapped, Packed in wooden cabins.

  • Duplex Steel Welded Pipe

    Duplex Steel Welded Pipe

    Type: Duplex Steel Welded Pipe, Duplex Steel Welded Tube
    Spec.: Outer Diameter: 6.0-630mm. Thickness: 0.5-45mm
    Standard: ASTM A790, A789, A815 / ASME SA790, SA789, SA815
    Grade: UNS S31803, UNS S32205
    End: Plain End, Beveled End, Treaded
    Packing: Waterproof paper wrapped, Packed in wooden cabins.

  • Carbon Steel Fittings

    Carbon Steel Fittings

    Type: Carbon Steel Seamless Fitting, Carbon Steel Welded Fitting, Carbon Steel Tee, Carbon Steel Reducer, etc.
    Bending Radius: R=1D, 2D, 3D, 5D, 6D, 8D, 10D or Custom
    Dimensions: ANSI/ASME B16.9, B16.28, MSS-SP-43.
    Grade: ASTM/ASME A234 WPB/A860 – MSS-SP-75 WPHY 42/46/52/56/60/65/70; A420 WPL3/A420 WPL6
    Range: ½”NB to 48″NB in Sch 10s, 40s, 80s, 160s, XXS.
    Packing: Waterproof paper wrapped, Packed in wooden cabins.

  • Stainless Steel Fittings

    Stainless Steel Fittings

    Type: Stainless Steel Seamless Fitting, Stainless Steel Welded Fitting, Stainless Steel Tee, Stainless Steel Reducer, etc.
    Bending Radius: R=1D, 2D, 3D, 5D, 6D, 8D, 10D or Custom
    Dimensions: ANSI/ASME B16.9, B16.28, MSS-SP-43.
    Grade: 201, 202, 304, 304L, 304H, 309S, 309H, 310S, 310H, 316, 316TI, 316H, 316L, 316LN, 317, 317L, 321, 321H, 347, 347H, 904L
    Range: ½”NB to 48″NB in Sch 10s, 40s, 80s, 160s, XXS.
    Packing: Waterproof paper wrapped, Packed in wooden cabins.